Peeled bars
Peeled bars from 17 to 80 mm.
Peeled bars from hot rolled bars can be produced with the following additional operations and controls:
- Heat treatment by annealing (soft and spheroidized annealing and so on)
- Heat treatment by quenching and tempering, normalising or stress reliving by induction
- Ends chamfering
- Surface defect control by Eddy Current
- Anti-mixing control
- Ultrasonic test
Peeled bars from hot rolled coil can be produced with the following additional operations and controls:
- Heat treatment by annealing (soft and spheroidized annealing and so on)
- Heat treatment by quenching and tempering, normalising or stress reliving by induction (after peeling)
- Ends chamfering
- Surface defect control by Eddy Current
- Anti-mixing control
Peeled bars from 17 to 80 mm.
Peeled bars from hot rolled bars can be produced with the following additional operations and controls:
- Heat treatment by annealing (soft and spheroidized annealing and so on)
- Heat treatment by quenching and tempering, normalising or stress reliving by induction
- Ends chamfering
- Surface defect control by Eddy Current
- Anti-mixing control
- Ultrasonic test
Peeled bars from hot rolled coil can be produced with the following additional operations and controls:
- Heat treatment by annealing (soft and spheroidized annealing and so on)
- Heat treatment by quenching and tempering, normalising or stress reliving by induction (after peeling)
- Ends chamfering
- Surface defect control by Eddy Current
- Anti-mixing control
Sales